Decals

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
jjh727
Posts: 2
Joined: Fri May 27, 2005 12:45 pm
Location: Massachusetts

Decals

Post by jjh727 »

I have been fusing jewelry for several years and now would like to try experimenting with decals.

I was wondering if I can be successful without having a controller on my kiln.

Any comments/suggestions and sources to purchase decals.

Thanks in advance.
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Decals

Post by Barry Kaiser »

Sure,
Decals come in high fire and low fire.
Just bring the temperature of your kiln to the level required by the type and turn off the kiln. You are done.
Note" if there is red or gold on the decal, vent(open the kiln lid slightly) it up to 1000°F.

Barry