Water drip system

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Water drip system

Post by Peter Angel »

I need a system that drips water onto a surface for cold working...the type of thing that comes standard with expensive cold working equipment.

I have been using a suspended bucket with a small hole in the bottom filled with water that slowly drip due to gravity. This works but i want to buy something less primitive :D

What's the correct term for this type of system?

Pete
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Water drip system

Post by Morganica »

I use loc-lines, plugged into a garden hose or an inside water supply: https://youtu.be/lJjlqjK7HOE

HIS Glassworks carries them here, not sure who might have them in your area.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Water drip system

Post by Buttercup »

Pete, if you can't find loc-line look in the gardening supplies section of a hardware store or a hydroponics supplier. They will have flexible irrigation tubing. You can get little on/off valves too. Locline works well. I just rigged something up from what we and a neighbour had handy.

http://www.accenthydroponics.com/index. ... ory_id=144

I have a 3 litre milk container on a shelf above the wet belt sander with an on/off valve at the bottom of the container where the flexible line is connected. It gravity feeds onto the belt. Jen
smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Re: Water drip system

Post by smallbitz »

I use the Loc-lines as well. They are super! Attached to a garden hose as Cynthia said, and then I just attach to my saw (grinder, etc.) with zip ties.
Terry Gallentine
Posts: 195
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: Water drip system

Post by Terry Gallentine »

I use small water supply pumps that are made for tile saws with a small inline valve for my water supplies. You can get the small pumps at Home Depot (around $20). One advantage is that you can use the pump to pump water out of a five gallon bucket instead of running a garden hose as your water source.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Water drip system

Post by Kevin Midgley »

belgium water feed for center feeding disc from belowhttp://covington-engineering.com/suppli ... ium-style/
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Water drip system

Post by Peter Angel »

Dear all. Thank you for the info. I have found lots of local sources of loc-line modular hose system. Pete