Page 1 of 1

2 way mirror

Posted: Mon Aug 24, 2015 11:46 am
by Bert Weiss
does anybody have experience kiln carving with 2 way mirror?

Re: 2 way mirror

Posted: Tue Aug 25, 2015 2:43 am
by Buttercup
Don't you love it when someone who's never done something offers advice :roll: ? I've never done it but my guess is that the silvering would fry/melt off, unless the kiln stays under the temperature that the molten tin would be when the glass is floated on it. Please report back if you try it. Jen