Borax or boric acid?

Post by Terry Gallentine »

Which is a stronger flux, borax or boric acid? Are there any other notable differences in the way they work between the two?
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Borax or boric acid?

Post by Bert Weiss »

All I know is that 20 mule team borax works. I never tried anything else. Some will crystalize at the bottom of the bottle, just pour the liquid off and it works. This stuff is cheap.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Borax or boric acid?

Post by charlie »

borax: Na2B4O7

boric acid: H3BO3

they are not interchangeable and not the same.