Page 1 of 1
					
				Patty Gray Mold
				Posted: Sat Sep 05, 2015 7:47 pm
				by Deb
				I just purchased one of the Patty Gray Dam Mold.   I kiln washed it and then found some instructions on the web that indicated to use boron nitrate.   Is kiln washed and then lining with shelf paper ok to use?
			 
			
					
				Re: Patty Gray Mold
				Posted: Sat Sep 05, 2015 8:18 pm
				by Marty
				Boron nitrate ain't.  You'll want boron nitride but if this is a ceramic mold then I don't know why kiln wash won't work.  Lining with shelf paper before firing will most likely get you a lump of crumpled fiberpaper in the bottom of the mold, stuck to the glass in ways you won't like.
However, I haven't gone through the tutorial........
			 
			
					
				Re: Patty Gray Mold
				Posted: Thu Sep 10, 2015 2:27 pm
				by JestersBaubles
				Love the PG Dam molds. Use them per the directions and you will have good success. That being said, I think kiln wash would be fine, but do line the bottom with Papyros or Thinfire.
2 cents,
Dana  W.
			 
			
					
				Re: Patty Gray Mold
				Posted: Sat Oct 10, 2015 1:51 pm
				by jim burchett
				Why not Ask Patty?