sharpie oil based paint marker survives taurus ring saw

Post by Peter Angel »

Hi all,

I've made a discovery!

The sharpie oil based paint marker stays put as you cut the glass using a Taurus ring saw.

No more vanishing lines.

All you need to do is wait 5 minutes for the marking to dry.

Have a look at the attached phone. It even stays put after you've cut it! (remove with a hard green plastic scrubbing sponge)

Pete

Attachments
sharpie oil based marker small.jpg
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: sharpie oil based paint marker survives taurus ring saw

Post by Peter Angel »

This is the sharpie oil based paint marker:

http://www.sharpie.com/en-US/oil-based- ... p-00030--1
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: sharpie oil based paint marker survives taurus ring saw

Post by Buttercup »

Interesting phone, which end do you speak into? :D

Thanks for the tip, Pete. Did you buy it in Oz? Jen
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: sharpie oil based paint marker survives taurus ring saw

Post by Bert Weiss »

If you don't clean off the marks and then fire the glass, the marks will disappear except for some place where it really ruins the design...