sharpie oil based paint marker survives taurus ring saw
Posted: Sat Sep 19, 2015 8:20 pm
Hi all,
I've made a discovery!
The sharpie oil based paint marker stays put as you cut the glass using a Taurus ring saw.
No more vanishing lines.
All you need to do is wait 5 minutes for the marking to dry.
Have a look at the attached phone. It even stays put after you've cut it! (remove with a hard green plastic scrubbing sponge)
Pete
I've made a discovery!
The sharpie oil based paint marker stays put as you cut the glass using a Taurus ring saw.
No more vanishing lines.
All you need to do is wait 5 minutes for the marking to dry.
Have a look at the attached phone. It even stays put after you've cut it! (remove with a hard green plastic scrubbing sponge)