Page 1 of 1
SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?
Posted: Sat Nov 28, 2015 6:05 pm
by JoanG
I've been full fusing 7 inch plates for years, using the same schedule. I use a small hot start kiln that doesn't allow much in terms of controlling the heat, ramp speed, etc. I use a tiny amount of glue to hold the top and bottom pieces in place. Suddenly there are "bubbles" under the top layer and the glass isn't firing flat for the full fuse. I'm not sure how to attach a photo but any ideas or suggestions would be GREATLY appreciated! Thank you.
Re: SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?
Posted: Mon Nov 30, 2015 9:05 pm
by Jordan Kube
Perhaps you've lost an element or they are getting old, etc.
Re: SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?
Posted: Mon Nov 30, 2015 11:41 pm
by Brad Walker
What schedule did you use? Is the top or bottom glass a different one that the one you've used in the past?
Does the kiln have top only elements or side and top?
Re: SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?
Posted: Wed Dec 23, 2015 12:15 am
by Emily Speight
is there any possibility that your shelf has a small dip in it? perhaps you were using one side and flipped it?
while it's a workaround, a very fine sifting of clear powder between the layers can help prevent bubbles.
i would like to see your schedule...