Fossils

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Post Reply
Jordan Kube
Posts: 18
Joined: Sun Oct 01, 2006 10:40 pm
Location: Seattle

Fossils

Post by Jordan Kube »

This is some of my new work. Pate de verre, System 96. I've been blowing glass for 18 years and got into kiln work in 2013. This board has been a great resource. Thanks everyone.

Archaeopteryx both 16" x 12" x .25"

Coelacanth fossil 12" x 8" x .25"
Attachments
Jordan_December2015_AlecMiller_ScreenSize-7 large resize.jpg
Jordan_December2015_AlecMiller_ScreenSize-8 large resize.jpg
Jordan_December2015_AlecMiller_ScreenSize-9 large resize.jpg
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Fossils

Post by JestersBaubles »

Nice. I really like the one in the middle.

Dana W.
AndyT
Posts: 170
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Fossils

Post by AndyT »

Very nice!! =D>
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Fossils

Post by Buttercup »

It must have been a thrill opening the kiln to those. Well done! Jen
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Fossils

Post by Peter Angel »

I like the fish!
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Post Reply