Vermiculite shelves source

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Vermiculite shelves source

Post by DonMcClennen »

Does anyone have a source for 1" or 2" sheets of vermiculite up to 24"x 48"? Canadian or USA .....thanks, Don
"The Glassman"
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Vermiculite shelves source

Post by Kevin Midgley »

ceramaguard is at every professional building drywall finishing supplier.
Yes it can warp unless supported as can any of these shelf materials.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Vermiculite shelves source

Post by Bert Weiss »

A great source for vermiculite boards is Jim Wiles in Charlotte NC
http://www.southernserviceco.com
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions