What temp is afap

Post by peterbr »

Here is a stupid question. The first segment is 300 per hour to 1350, then segment 2 is Afap to 960. What temp do I set the kiln at to go afap to 960.

Thanks
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: What temp is afap

Post by Brad Walker »

For most controllers, it's 9999, which is as fast as can be programmed.