Imprints/Flat slumping
Posted: Sun Feb 21, 2016 6:00 pm
Hello!
I have a project on some large sheets of glass (float, 50x50"). I need to imprint on dry plaster and fire 2 sheets at once. What can I use for the bed and what kind of separator between sheets?
Devit problems?... and a fire schedule for an electric kiln...
I have in my studio whiting, kaolin, alumina hydrate, quarz sand, plaster of Paris
Thanks!
I have a project on some large sheets of glass (float, 50x50"). I need to imprint on dry plaster and fire 2 sheets at once. What can I use for the bed and what kind of separator between sheets?
Devit problems?... and a fire schedule for an electric kiln...
I have in my studio whiting, kaolin, alumina hydrate, quarz sand, plaster of Paris
Thanks!