CLOUDY BOTTLES.......HELP PLEASE!!!!!
Posted: Fri Feb 20, 2004 5:12 pm
by lanie
Hello, Can anyone help me please.......I melt bottles in my kiln and am having a problem with them being cloudy when they are done, can anyone tell me how to avoid this problem? I also use decals on them so I need something that won't ruin the decal. I have heard about something called SPRAY A and BORAX, if either of these would help how would I use them? Also I use these bottles for food after they are done, would this cause a problem in any way??????
Posted: Sat Feb 21, 2004 9:00 am
by Luiza
Hi lanie
I do this all the time, just put a spoon of Borax in half a cup of warm water, brush the half of the bottle yhat won´t touch the shelf and wait till it´s dry (few minutes, if the water is warm). You can brush over the decals, if they are already dry, no problems. You just can´t let the borax touch the side of the bottle that will touch the shelf...
I use to do it in two times, cause my decals fire at 720 degrees celcius. I fuse the bottle, without borax, no matter it´s cloudy... Then I apply the decal and it goes again to the kiln. I do a kind of pot to snaks with some of my bottles, so I fire them with the decal over a mould.
Hope I was clear, my english is not so good
The right forum for this question is the Kiln-forming Discussion...
Big hug
Luiza
Posted: Sat Feb 21, 2004 12:52 pm
by whitejoyce
Hi ladies,
I want to do something more with my bottles, can I ask for more suggestions from you, I mean other than the cheese tray's & ash tray's.
What do you do with your bottles?
Thanks in advance for any suggestions
Posted: Sat Feb 21, 2004 11:57 pm
by whitejoyce
Hi Lanie,
I tried to send you email address. whitejoycox.net
about more on how to create with the bottles.
Hope you understand,
Posted: Sun Feb 22, 2004 9:37 am
by Luiza
whitejoyce wrote:Hi Lanie,
I tried to send you email address. whitejoycox.net
about more on how to create with the bottles.
Hope you understand,
Please, send it to me too.
glass1@uol.com.br
Thanks
Luiza
Posted: Sun Feb 22, 2004 6:24 pm
by Pat Loboda
I'd like to have the ideas for bottles, too, please.
pat@glassbypat.com
Thanks in advance,
Pat Loboda
Posted: Thu Feb 26, 2004 12:04 pm
by tel
Hi J White
I'd love to have that information as well if you don't mind sending it to me. I'd appreciate it.
Thank you Tess
tlilly@innoqual.com 
Bottles
Posted: Thu Feb 26, 2004 2:11 pm
by Kay
Would you add me to your list?
Thanks!
Kay
TomKayC@aol.com
Posted: Thu Feb 26, 2004 3:11 pm
by Brad Walker
Please, please, please, if you want to contact someone do it via email or via private message, rather than posted on the board.
To do this, simply click on the button that says "PM" (for "private message" or "Email" (for "email") that's at the bottom of every post on the board. That will send either a message or an email directly to the poster. It also frees up disk space on the board for glass discussion and topics.
Another advantage of doing this is that it keeps everyone's email address private, rather than posted on a public forum. If you post your email address publicly, then you are increasing the likelihood that it will be harvested and used to send you spam. If you click on the PM or Email button, the addresses stay private and can't be harvested.
Thanks for understanding.