Wissmach colours

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Wissmach colours

Post by DonMcClennen »

Anyone know why Wissmach 96 has so few opal colour choices? Mostly greens and blues... don't see any red, orange, purple.. etc. Are they going to add more any time soon :?: Dwindling Spectrum inventories are creating a need!
"The Glassman"
AndyT
Posts: 170
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Wissmach colours

Post by AndyT »

They have come out with more opals. Not sure about the purple yet.
wiss.jpg
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Wissmach colours

Post by JestersBaubles »

They have a medium-colored purple opal, it's named "Violet". The sample on the web site, at least on my computer, looks grey, but it's a medium lilac color.

Dana W.
Post Reply