Page 1 of 1
Wissmach colours
Posted: Wed Sep 14, 2016 2:17 pm
by DonMcClennen
Anyone know why Wissmach 96 has so few opal colour choices? Mostly greens and blues... don't see any red, orange, purple.. etc. Are they going to add more any time soon

Dwindling Spectrum inventories are creating a need!
Re: Wissmach colours
Posted: Thu Sep 15, 2016 11:54 am
by AndyT
They have come out with more opals. Not sure about the purple yet.
Re: Wissmach colours
Posted: Sun Sep 18, 2016 12:43 am
by JestersBaubles
They have a medium-colored purple opal, it's named "Violet". The sample on the web site, at least on my computer, looks grey, but it's a medium lilac color.
Dana W.