Spectrum 96
Posted: Wed Mar 29, 2017 2:54 pm
				
				Has anyone heard any news about 96 glass being available and when. I also heard there maybe someone else besides oceanside
			Guide to fusing, slumping, and related kilnforming techniques
https://warmglass.com/phpBB3/
Wissmach is coming out with new colors and it will be a while before any Spectrum is being produced although it appears most distributors have a fair amount on hand.BobbieMatus wrote:Has anyone heard any news about 96 glass being available and when. I also heard there maybe someone else besides oceanside