Hello ! Please can anybody give me a schedule for firing and slumping a bowl of Car window Glass (I hope I use the right words in English for this material

) Thank you, Jan from Holland
Re: Car window glass
Posted: Wed Apr 26, 2017 4:38 pm
by DonMcClennen
Car window glass use to be 2 thin layers of a glass sandwich with a thin plastic layer in the middle. If this is still the way its made then fusing is not an option..
Re: Car window glass
Posted: Thu Apr 27, 2017 11:22 am
by Rick Wilton
Car WINDOWS are tempered....... car windshields are laminated.
Windows good to fuse
Windshields NOPE
Re: Car window glass
Posted: Fri May 12, 2017 5:47 am
by Jan de Jong
Rick Wilton wrote:Car WINDOWS are tempered....... car windshields are laminated.
Windows good to fuse
Windshields NOPE