Spectrum System 96
Moderators: Brad Walker, Tony Smith
-
susanmozingo
- Posts: 7
- Joined: Sun Jun 06, 2004 4:12 pm
Spectrum System 96
How can you tell which side is the top side of a clear sheet of System 96?
Re: Spectrum System 96
If you have any seeds in it they are on the bottom. also, the back side usually has a slight matte look.susanmozingo wrote:How can you tell which side is the top side of a clear sheet of System 96?
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Spectrum System 96
I don't think there is really a "top" side. There is a smooth side and a side that is a bit textured. Depending upon what you are doing dictates which side is facing up.
For instance, when layering glass pieces, I will try to put texture facing texture, or at least texture facing smooth to minimize bubbles (smooth to smooth is when you'll more likely get bubbles).
Best, Dana
For instance, when layering glass pieces, I will try to put texture facing texture, or at least texture facing smooth to minimize bubbles (smooth to smooth is when you'll more likely get bubbles).
Best, Dana
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Spectrum System 96
The side that has the label is the "top" side.
The other Jim
The other Jim
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: Spectrum System 96
Jim is right, but keep in mind that art glass isn't like float glass which has one side "contaminated" by the float process.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Spectrum System 96
Tony.
By "contamination" I assume that you mean the tin left by the float process.
The other Jim
By "contamination" I assume that you mean the tin left by the float process.
The other Jim
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: Spectrum System 96
Yup. That's what I meant, and why most people ask which side is up.jim simmons wrote:Tony.
By "contamination" I assume that you mean the tin left by the float process.
The other Jim
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun