Reduce/remove micro bubbles in full fused pieces
Posted: Wed Nov 15, 2017 2:31 pm
				
				Looking for suggestions -
I've been working on simple full fused tiles - 2 layers, one being clear. I end up with micro bubbles in the finished piece. Happens with two pieces directly on top of one another, and when I put small clear "chads" under the corners of the top layer. So suspect it is my schedule. I'm using a 150/hour ramp from 900 to 1100, holding 1100 for 30 minutes, then a 250/hour ramp to 1500, holding for 30 minutes before heading back down AFAP to 900 for a 1 hour hold. Any thoughts as to how can adjust anything at all to have a more pristine finished tile?
Also, any thoughts as to a remedy for the fused tiles that have the bubbles - is refusing an option?
			I've been working on simple full fused tiles - 2 layers, one being clear. I end up with micro bubbles in the finished piece. Happens with two pieces directly on top of one another, and when I put small clear "chads" under the corners of the top layer. So suspect it is my schedule. I'm using a 150/hour ramp from 900 to 1100, holding 1100 for 30 minutes, then a 250/hour ramp to 1500, holding for 30 minutes before heading back down AFAP to 900 for a 1 hour hold. Any thoughts as to how can adjust anything at all to have a more pristine finished tile?
Also, any thoughts as to a remedy for the fused tiles that have the bubbles - is refusing an option?