cutting a mulite kiln shelf with a skill saw

Post by jim simmons »

Can I cut a mullite kiln shelf with a skill saw without ruining the saw blade?
The other Jim
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: cutting a mulite kiln shelf with a skill saw

Post by Kevin Midgley »

wet shelf diamond blade
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: cutting a mulite kiln shelf with a skill saw

Post by DonMcClennen »

Use a blade made for concrete or ceramics.
"The Glassman"