firing schedule

Post by traceynsv »

HI All,

I have a water scene that I have already fired, B.E. .clear,with frits size is 12 x 6 Now I want to put that on top of B.E. 4200
do I add more soak time and ramp up slower?

Thanks, Tracey
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: firing schedule

Post by Brad Walker »

Yes, absolutely. Slower up and longer anneal on the way down.