Sink or not sink??!!

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Bozurka Pejcic
Posts: 5
Joined: Mon Sep 22, 2003 4:05 pm
Location: Seattle,WA

Sink or not sink??!!

Post by Bozurka Pejcic »

Hi everyone,

A while ago you were so nice to answer my question about setting up a new glass studio even though it was answered many, many, times before. :oops: I wanted to show appreciation for your patience, again.
Thanks to you and to absolutely incredible source of information that is in the archive I was able (even with still very limited knowledge of fusing process), to come up with floor plan for my new basement studio.
Was it successful we will see in a year or two…. 8-[

We are in construction phase now and I still have couple of questions. I looked carefully through archive and could not fined an answer….
Brock has mentioned that nice darkroom plastic sink, wide but shallow is something useful to have. We are adding a toilet and kitchenette, so I am planning to add this utility sink as well. It would be a part of my “dirty roomâ€
Bozurka, Seattle
Post Reply