Page 1 of 1
Making small pieces glass
Posted: Tue May 14, 2019 6:47 am
by Jan de Jong
Hello ! I know the manner to make small pieces glass bij heating the glass and throw it in cold water. Now I wonder....if I do this for a second/third time will the glass-parts become smaller every time? Thank you ! Jan de Jong (Holland)
Re: Making small pieces glass
Posted: Wed May 15, 2019 6:45 am
by Jan de Jong
Perhaps I did give to little information as there is no reaction ? Heating up the glass and throwing in cold water is to make frit. But the measurement is still too big for me.
So I wonder if I can do it again to get smaller parts ? Jan de Jong
Re: Making small pieces glass
Posted: Wed May 15, 2019 8:41 am
by Ed Cantarella
They'll resist getting smaller as the smaller pieces can take the stress better or just plain have less of it. You'll need to crush or grind it beyond that. If you get a crusher, I'd suggest you get one with a sturdy, solid handle(not the Aanraku) and instead of pumping up and down, put it on a solid surface and strike the handle with a hammer 3-4 times. Hitting more times is pointless, the glass will compact and is very strong. Pour out into a screen and throw the bigger pieces back in the crusher, repeat. * If you pump the handle up/down you are pumping lots of fine glass dust into the air.
A few people are making crushers and selling on ebay . . . I have one made by
baleak@live.com
It is the "Sore Thumb Rock Crusher"

Very plain but very sturdy.
Re: Making small pieces glass
Posted: Wed May 15, 2019 12:29 pm
by Jan de Jong
@ Ed Cantarella: Thank you for your answer ! But....I wish not to make "frit". When you heat the glass and throw it in cold water, there are made nice round little pieces.
But I wish this pieces still smaller and wonder how to do. So I thought: once again heating and in cold water these pieces. If nobody knows if this will work I have to test it myself. greetings from Holland, Jan
Re: Making small pieces glass
Posted: Wed May 22, 2019 11:49 pm
by Don Burt
Jan, did you perform the experiment? What was the result?
Re: Making small pieces glass
Posted: Sun Jul 14, 2019 4:29 am
by Jan de Jong
@ Don Burt: Sorry for my late respons ! No, I did not test as I heard from a fuser that this pieces will not become smaller. Jan