Post by Michael Stevens »

Instead of casting a complete round piece. i thought if I made a mold that was half round and glued 2 pieces together would the seem be visible? any glues that have better result? the epoxy resin I get here has an odor for about a month
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: gluing question Long round twisting pieces

Post by Brad Walker »

Regardless of the glue used, the seam would be visible.