Post by Michael Stevens »

I made some molds from shells as casted them, they have nice texture if I tack fuse to a project will the texture be flattened. Or is the only solution to glue. them on?

I guess I could use powdered glass and paint the details to look like the pattern. but I was hoping to. keep the original pattern, my daughter collected. these shells so I wanted a special piece.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: keeping Texture on glass

Post by Brad Walker »

If you tack fuse at a low enough temperature you'll keep most of the texture. 1350F/730C is high enough to stick glass together and retain most of the texture. The higher above that you go, the more texture you will lose.
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: keeping Texture on glass

Post by Barry Kaiser »

Use a low temperature flux, or a glass paint as a glue. I've done a lot of these.