Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

frit lace rescue

Post by Michael Stevens »

It seems a little light and if I remove it from. the kiln shelf there will be pieces fall off. can you cap it and refire it without changing kiln paper.
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: frit lace rescue

Post by jim simmons »

as long as the paper is not torn or disturbed and you can not see the kiln shelf, you can reuse it.
The other Jim
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

Re: frit lace rescue

Post by Michael Stevens »

Thanks Jim. saves a lot of tedious work rearranging little frit mounds by hand. I. wish I. had a long handled spoon so I could drop some extra frit during firing in case some areas are lighter.
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: frit lace rescue

Post by jim simmons »

Hey, Michael.
Would you be so kind as to let us know how your 2nd firing on the kiln paper turned out?
Thanks.
The other Jim
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

Re: frit lace rescue

Post by Michael Stevens »

came out ok. a little extra texture on the back. needed a little more cold working. but it's ok.
IMG_20200827_122248.jpg
overall I'm. satisfied
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: frit lace rescue

Post by The Hobbyist »

Nice job...well done!

Jim "The Hobbyist"