Page 1 of 1
frit lace rescue
Posted: Mon Aug 24, 2020 9:43 am
by Michael Stevens
It seems a little light and if I remove it from. the kiln shelf there will be pieces fall off. can you cap it and refire it without changing kiln paper.
Re: frit lace rescue
Posted: Mon Aug 24, 2020 12:23 pm
by jim simmons
as long as the paper is not torn or disturbed and you can not see the kiln shelf, you can reuse it.
The other Jim
Re: frit lace rescue
Posted: Wed Aug 26, 2020 2:16 am
by Michael Stevens
Thanks Jim. saves a lot of tedious work rearranging little frit mounds by hand. I. wish I. had a long handled spoon so I could drop some extra frit during firing in case some areas are lighter.
Re: frit lace rescue
Posted: Sat Aug 29, 2020 12:24 pm
by jim simmons
Hey, Michael.
Would you be so kind as to let us know how your 2nd firing on the kiln paper turned out?
Thanks.
The other Jim
Re: frit lace rescue
Posted: Sun Aug 30, 2020 9:11 pm
by Michael Stevens
came out ok. a little extra texture on the back. needed a little more cold working. but it's ok.
overall I'm. satisfied
Re: frit lace rescue
Posted: Mon Aug 31, 2020 8:54 am
by The Hobbyist
Nice job...well done!