COE 90 frit balls ok on COE 96 Christmas trees?
Posted: Sun Aug 30, 2020 1:11 pm
by conboc
I just glued a batch of COE 90 frit balls to flat 6mm Christmas trees made from COE 96 glass. Oops. Does anyone know I might be able to get away with firing these? The dark shadows are gold decals I intended to fire to 1350 for 11 minutes, with the frit balls.
Thank you.
Re: COE 90 frit balls ok on COE 96 Christmas trees?
Posted: Sun Aug 30, 2020 9:09 pm
by Michael Stevens
you might be able to tack fuse, but really it could crack later. personally, I'd make compatible frit bslls
Re: COE 90 frit balls ok on COE 96 Christmas trees?
Posted: Mon Aug 31, 2020 8:57 am
by Barry Kaiser
I use a little bit of my paints....just a dot, to attach the balls. This seems to act as a buffer for the differing COEs.
Remember the contact area is very small.