I found this question here from long ago, but there was no response.
Boron Nitride spray is used as seperator on RVS.
But there is also POWDER. Had anyone try this ?? Jan
Boron Nitride POWDER
Moderator: Tony Smith
-
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
-
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Boron Nitride POWDER
Mix the powder with water to a cream consistency and paint it on like you would kiln wash.
I have used it on SS and clay fired stuff with good results.
The other Jim
I have used it on SS and clay fired stuff with good results.
The other Jim
-
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Boron Nitride POWDER
@ Jim Simmons: Thank you for your reply !! Do you heat the SS ( and Clay fired) ?? Jan
-
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Boron Nitride POWDER
nope. treat it just like it is a product called "ZYP".
paint it on, let it dry for about 30 min. and you are good to go.
The Other Jim
paint it on, let it dry for about 30 min. and you are good to go.
The Other Jim
-
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Boron Nitride POWDER
@ Jim: Thank you ! I PM you for another question. Jan