Hello, not knowing about this notation of COE. I think it is COE 96 ....am I right ?
COE (9,60 +- 0,15) x 10 -6 Sorry, don 't know how to make this signs in the right way. Jan
Reading COE
Moderator: Tony Smith
-
- Posts: 129
- Joined: Sun Jun 08, 2003 5:27 pm
- Location: East Tennessee
Re: Reading COE
Hi Jan. When I read your question, I thought this should be easy to find with Google. It was not, because the actual measurement has been lost to the reduced reporting of 90, 96, 82. etc. I finally found the answer in an earlier post on the board:
http://warmglass.com/phpBB3/viewtopic.php?t=41565
Look at the very bottom of the thread. So, 9.6x10-6 is the same as 96x10-5 and 96 COE, I think.....
http://warmglass.com/phpBB3/viewtopic.php?t=41565
Look at the very bottom of the thread. So, 9.6x10-6 is the same as 96x10-5 and 96 COE, I think.....
Lynn Perry
-
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Reading COE
@ Lynn Perry: Thank you ! Jan