				Reading COE
				Posted: Sat Nov 07, 2020 10:06 am
				by Jan de Jong
				Hello,  not knowing about this notation of COE. I think it is COE 96 ....am I right ?
COE (9,60 +- 0,15) x 10  -6         Sorry, don 't know how to make this signs in the right way.  Jan
			 
			
					
				Re: Reading COE
				Posted: Sat Nov 07, 2020 11:34 am
				by Lynn Perry
				Hi Jan.  When I read your question, I thought this should be easy to find with Google.  It was not, because the actual measurement has been lost to the reduced reporting of 90, 96, 82. etc.  I finally found the answer in an earlier post on the board:
http://warmglass.com/phpBB3/viewtopic.php?t=41565
Look at the very bottom of the thread.  So, 9.6x10-6 is the same as 96x10-5 and 96 COE, I think.....
 
			 
			
					
				Re: Reading COE
				Posted: Sat Nov 07, 2020 12:23 pm
				by Jan de Jong
				@ Lynn Perry: Thank you  !   Jan