Posted: Sun Feb 21, 2021 4:45 pm
				
				Hi - I am finally getting back to kilning after a 20 year hiatus!!  So my question deals with a stainless steel flower former (which the glass drapers over).  It has corroded after sitting in the garage for 20+ years.  Should this concern me?  I would plan to use kiln wash on the mold, but didn't know if there was anything else I should do. whether sanding it would only worsen the problem. Any thoughts would be appreciated.