Posted: Thu Apr 08, 2021 9:28 am
by Jan de Jong
Hallo, did see on a site heatresistant tape which was used by fusing. I marked the site as Favorite to look on it later.
Something went wrong.....no favorite and no idea where to search.
So my question is: is there tape with which you can fuse ?
Jan
Re: Heat resistant Tape
Posted: Thu Apr 08, 2021 10:41 am
by Brad Walker
So what are you wanting the tape to do?
Re: Heat resistant Tape
Posted: Thu Apr 08, 2021 12:45 pm
by Jan de Jong
@ Brad Walker: Instead of Ceramic felt between RVS and the glass. I saw somebody use it on Internet. For Full fuse . Jan
Re: Heat resistant Tape
Posted: Thu Apr 08, 2021 1:31 pm
by Brad Walker
That makes sense, just not sure why it would be better than fiber paper.
Most high temperature tape that I'm aware of is only rated to 500F, but might hold up longer insulated by glass. Google high temperature tape.