Smooshing Weights

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Smooshing Weights

Post by Don Burt »

Are flat iron griddles or 1/4 stainless steel plate suitable for using to press down glass in the kiln? Or will they spall and warp or something? The high end of the process is >1500F with a 30 minute hold. I don't want to ruin the metal just to find out its a bad idea. I can source some refractory shelves and bricks and stuff.

Brad's PDF downloadable here about smooshing is helpful. I'm having fun with mini-kiln sized pieces so far.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Smooshing Weights

Post by Buttercup »

Hi Don,

Can't answer your question but it's a long time without an answer so I thought I'd say 'Hi'! :lol:
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Smooshing Weights

Post by Don Burt »

HI Jen. Thank you for checking in. We could talk about AU women's swimming or something. They did well in Tokyo and in a time zone where their fans could actually watch it.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Smooshing Weights

Post by Buttercup »

Yes, they did shine. A little bit of good news among all the terrible news. I must admit I didn't watch any of the Games, just the highlights on the evening news.

When do we see a new glass masterpiece, Don? Your audience is waiting. No pressure........
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Smooshing Weights

Post by jim burchett »

Don, if you ha ent used the metal yet, I use kilnsjdlves and other refractory materials to provide the weight
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Smooshing Weights

Post by Buttercup »

Don, you wrote:
Brad's PDF downloadable here about smooshing is helpful. I'm having fun with mini-kiln sized pieces so far.
[/quote]

Don, or Brad, where can I find this PDF please?
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Smooshing Weights

Post by Don Burt »

Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Smooshing Weights

Post by Buttercup »

Thanks very much, Don.