Page 1 of 1
Silver Fuming
Posted: Fri Sep 03, 2021 5:42 pm
by jim burchett
I have made pieces in the past with Silver foil on BE reactive Ice and gotten a nice fume pattern. I am wondering if I use Tekta and Reactive Ice powder with Silver it will give a similar effect?
Re: Silver Fuming
Posted: Fri Sep 03, 2021 6:19 pm
by Brad Walker
Silver needs to be on top for best results, but would work.
Re: Silver Fuming
Posted: Fri Sep 03, 2021 6:49 pm
by jim burchett
Thanks, I always put the silver on top, I will run a cpl of text tiles tonight.
Re: Silver Fuming
Posted: Fri Sep 03, 2021 8:06 pm
by Brad Walker
jim burchett wrote:text tiles
Test me the results.

Re: Silver Fuming
Posted: Sat Sep 04, 2021 12:28 pm
by jim burchett
While it did react, and there was some Halo, it wasn't nearly as intense as on the glass itself. Tried several different thicknesses of the powder, but it distorted the transparency in relation to its depth. So, these will just cost more in the future. So the answer is Yes, but....
Re: Silver Fuming
Posted: Wed Sep 08, 2021 1:47 pm
by jim simmons
Maybe try to fuse the powder first then refuse with the silver?
The oher Jim
Re: Silver Fuming
Posted: Thu Sep 16, 2021 5:33 pm
by jim burchett
Too many steps then