slump 17x11 piece 5/16” thick over ceramic wave mold.
Posted: Sun Dec 26, 2021 10:47 pm
I am using a Bullseye double curved ceramic mold size 17x11. The glass is 5/16” thick. I think the annel should be for 2 or 3 hours T 900 degrees F.
1. 50f to 300f .hold 15 minutes
2. 100f to 800f hold no hold
3. 150 f to 1000F hold 5 minutes
4. 100 F to 1215F hold 10-15 minutes visually check
5. 600f to 900f hold for 2 or 3 hrs?
6. 200f to 800f. hold 01. minute
7. 100F to 500f hold 01. minute
8. 250f to 80f hold 00
I have never tried to slump a piece this thick. Does the schedule seem close.?
I think I will need to visually check the slump
Thanks for any assistance.
Carol Ann
1. 50f to 300f .hold 15 minutes
2. 100f to 800f hold no hold
3. 150 f to 1000F hold 5 minutes
4. 100 F to 1215F hold 10-15 minutes visually check
5. 600f to 900f hold for 2 or 3 hrs?
6. 200f to 800f. hold 01. minute
7. 100F to 500f hold 01. minute
8. 250f to 80f hold 00
I have never tried to slump a piece this thick. Does the schedule seem close.?
I think I will need to visually check the slump
Thanks for any assistance.
Carol Ann