Page 1 of 1
best glass for toppping
Posted: Wed Mar 30, 2022 1:40 pm
by Birdzilla44
Any suggestions for a clear glass (Bullseye coe 90) as a fused topping glass? Need clear and no bubbles.
Re: best glass for toppping
Posted: Thu Mar 31, 2022 5:24 pm
by david n
I use 3mm Tekta clear to cap all of my work. Bullseye also makes crystal clear Tekta, but the regular works well for me. Occasionally I find bubbles that I don't like and I will just drill them out and use the piece on a different layer of my work.
Re: best glass for toppping
Posted: Fri Apr 01, 2022 4:22 pm
by Birdzilla44
Thanks David. I have not tired the crystal clear tekta, but if the difference is negligible in clarity and lack of color, the regular should work for me. A good shiny clear is want I want.