Fusing 5mm clear sheets
Posted: Tue Jun 21, 2022 8:09 pm
Hi,
I am running out of COE 96 casting plates and cannot find anymore. Sadness.
My castings are 6 to 7 feet tall and about 1.5 thick with frit on the surface of the mold.
Thinking of fusing 8 layers of 5mm clear sheets together.
Is this crazy or worth a try?
Appreciate any thoughts or info your can share,
Thanks, Peter
I am running out of COE 96 casting plates and cannot find anymore. Sadness.
My castings are 6 to 7 feet tall and about 1.5 thick with frit on the surface of the mold.
Thinking of fusing 8 layers of 5mm clear sheets together.
Is this crazy or worth a try?
Appreciate any thoughts or info your can share,
Thanks, Peter