Grinding

Post by Janet Ostinelli »

Had to grind small spot after full fusing. Do I need to fire polish the dull spot before slumping or will the slump firing take care of it
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Grinding

Post by Kevin Midgley »

depends how much roughness there is or if you have hand polished it to smooth. 220 grit could get you close. Warning the slightest amount of grinding residue will show up. Keep wet and clean well.