Anneling kiln for fusing?

Posted: Thu Jun 15, 2023 12:11 pm
by Bonnie Rubinstein
Hi All,
I know someone who has a few annealing kilns for use by glass blowers. He wonders if they could also be used for fusing. I am not familiar with annealers.
Can they be also used for fusing?
Thanks!

Re: Anneling kiln for fusing?

Posted: Thu Jun 15, 2023 12:56 pm
by Mark Hughes
It should as long as it will fire to the processing temps you need for your work. The Skutt ones I looked at had a top temp of 1700*, which is higher than you need for Bullseye glass.

Re: Anneling kiln for fusing?

Posted: Thu Jun 15, 2023 7:44 pm
by Bonnie Rubinstein
Thank you. he said it does go to 1400.

I should probably check to see what his controller looks like.