Clear/ smooth 90 COE glass

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
LCS
Posts: 8
Joined: Mon Aug 20, 2007 9:44 am

Clear/ smooth 90 COE glass

Post by LCS »

I have used clear/smooth 90 COE glass for many years for most of my projects, especially to cap cabochons. I have been told it is no longer being produced. What is the alternative?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Clear/ smooth 90 COE glass

Post by Brad Walker »

I suspect the "clear/smooth 90 COE glass" you're referring to is the machine rolled clear that Uroboros used to make. It's true, that's no longer being made.

However, you could use the regular Bullseye clear just fine. Even though it's not as smooth, it will do just as good a job of capping cabochons. Just hold for half an hour or so at 1230F on the way up.
Post Reply