Page 1 of 1
Kiln Question
Posted: Sat Aug 19, 2023 12:57 pm
by Mark Hughes
I am finally getting back to fusing after a long break.
Is there anything I need to check before I test my kiln ( Glass Glow) after not using it for 10 years? It's got a nice Paragon controller that I don't want to mess up!

Re: Kiln Question
Posted: Sat Aug 19, 2023 1:03 pm
by Don Burt
I have no suggestions. But welcome back!
Re: Kiln Question
Posted: Sat Aug 19, 2023 3:58 pm
by Brad Walker
Mark Hughes wrote: ↑Sat Aug 19, 2023 12:57 pm
I am finally getting back to fusing after a long break.
Is there anything I need to check before I test my kiln ( Glass Glow) after not using it for 10 years? It's got a nice Paragon controller that I don't want to mess up!
Put some scrap glass in it. Small pieces, two layers thick, in various places in the kiln. Fire to a full fuse and see what happens. It will tell you if the kiln is working fine and if it heats uneven.
Re: Kiln Question
Posted: Mon Aug 21, 2023 1:23 pm
by Mark Hughes
Thank you very much for the info!