Does anyone know if glass becomes less stable the more times it’s fired to 1600?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Used glass

Post by Brad Walker »

It will.