Amaco Glass
Moderators: Brad Walker, Tony Smith
-
Eric Bloom
- Posts: 8
- Joined: Fri May 15, 2020 3:39 pm
Amaco Glass
Has anyone used Amaco glass? I found several sample boxes, its all marked COE 90. I use 96. I've done a few firings with the Amaco using a schedule that works for 96 (not mixing the 90 and 96) and so far so good. I suspect this stuff is old.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Amaco Glass
You're right, it's really old stuff, 10 to 15 years old.
For a short period back then Amaco had a fusible line, but it didn't last long. Not sure if it was made by Bullseye or someone else, but it's 90COE, just don't mix it with your 96.
For a short period back then Amaco had a fusible line, but it didn't last long. Not sure if it was made by Bullseye or someone else, but it's 90COE, just don't mix it with your 96.