Page 1 of 1
Amaco Glass
Posted: Fri Aug 02, 2024 4:46 pm
by Eric Bloom
Has anyone used Amaco glass? I found several sample boxes, its all marked COE 90. I use 96. I've done a few firings with the Amaco using a schedule that works for 96 (not mixing the 90 and 96) and so far so good. I suspect this stuff is old.
Re: Amaco Glass
Posted: Fri Aug 02, 2024 10:16 pm
by Brad Walker
You're right, it's really old stuff, 10 to 15 years old.
For a short period back then Amaco had a fusible line, but it didn't last long. Not sure if it was made by Bullseye or someone else, but it's 90COE, just don't mix it with your 96.