rescue magnetic backing flat lap disc

Posted: Fri Oct 11, 2024 2:10 am
by Marian
The magnetic backing on my 24 inch diamond disc is coming off. Any advice to re attach? Separately, I got a new disc with no backing at all, just steel. Any way to put a magnetic sheet on that? Did I learn my lesson to read the description more carefully? I'm thinking of attempting contact adhesive and a roll of magnetic sign material as I can't return it.

Re: rescue magnetic backing flat lap disc

Posted: Mon Oct 14, 2024 3:37 pm
by Marty
That's exactly what you do- contact cement for the separation and new mag for the other.

Re: rescue magnetic backing flat lap disc

Posted: Mon Oct 14, 2024 4:38 pm
by Marian
Thanks! Ok, ordered the magnet sheet.