Page 1 of 1

Can I use hot glue in my kiln?

Posted: Sat Nov 09, 2024 5:37 pm
by Linda Jean
I’m making some Christmas decorations with my grandchildren and we have glued glass strips together to make stars with hot glue. They aren’t great works of art so I’m not too concerned how they will look, just want them to hold together to get them into the kiln. My concern was that the glue residue may harm the elements on the kiln in some way. Just wanted to check before I fire them. Thought?

Re: Can I use hot glue in my kiln?

Posted: Sat Nov 09, 2024 10:48 pm
by Brad Walker
Yes, you can use hot glue, just don't overdo it.

Re: Can I use hot glue in my kiln?

Posted: Sun Nov 10, 2024 4:54 am
by Linda Jean
Thanks Brad, what’s going to happen if you overdo it? Just concerned about the residue harming the kiln. Thanks. ☺️

Re: Can I use hot glue in my kiln?

Posted: Sun Nov 10, 2024 8:02 am
by Brad Walker
There won't be any harm to the kiln. The worst thing that can happen is that you get little black carbon spots on the glass.

Re: Can I use hot glue in my kiln?

Posted: Sun Nov 10, 2024 4:42 pm
by Linda Jean
Thanks so much. Will see how it goes!