Hole in glass using Patty Gray dam
Posted: Tue Nov 26, 2024 5:56 pm
Hi,
I emailed Patty but have not received a response. So, I am trying here. I use Patty's 8x10" dam a lot. All the first pieces I've made came out well. The last two pieces have big holes and bubbles in them. I use papyrus as she taught me in her class and store my molds in their original boxes. Please see pics and advise what may have gone wrong. Thank you!
Ginni
I emailed Patty but have not received a response. So, I am trying here. I use Patty's 8x10" dam a lot. All the first pieces I've made came out well. The last two pieces have big holes and bubbles in them. I use papyrus as she taught me in her class and store my molds in their original boxes. Please see pics and advise what may have gone wrong. Thank you!
Ginni