Page 1 of 1

Clean Burning Tape

Posted: Sat Jun 07, 2025 9:43 am
by Terry Gallentine
I have a need for a tape that I can temporarily tape glass pieces together before fusing. I have seen in older posts, the use of Scotch tape but I was wondering what the current information is regarding this. Is there something new that is better than Scotch tape?

Re: Clean Burning Tape

Posted: Sat Jun 07, 2025 9:25 pm
by Brad Walker
We've had good luck with both scotch tape and clear packing tape. Just don't lay it on too thick.

Re: Clean Burning Tape

Posted: Wed Jun 11, 2025 5:26 pm
by Terry Gallentine
I will give the scotch tape a try. Thanks Brad.