cracks in kiln bricks

Post by Gabriel »

Is it normal for kiln bricks to crack, nothing large, just small fissures that run for a few inches?
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Yup. Brock